We are in a position to supply fine and super fine reclaimed rubber, the main technical specifications as follows:
Grade One:
1.Superfine 2.Stretch intensity9.5mpa 3.Stretch rate:390%
Grade Two:
1.Superfine 2.Stretch intensity8.0mpa 3.Stretch rate:350%
Grade Three:
1.Superfine 2.Stretch intensity6.0mpa 3.Stretch rate:320%
Grade Four:
1.Superfine 2.Stretch intensity5.0mpa 3.Stretch rate:300% |
|
|
|
|